Denton Discovery 18

Tool Owner

Jim Pierce (jim.pierce@utah.edu)

Asset Number = , MAC = N/A, Port # = N/A, Serial # = 18003, Room # = Bay F

Reservations Calendar

  • Sputter deposition of metals, alloys, and insulating thin films (user configurable)
  • Film thicknesses controllable from a few nm to hundreds of nm
  • Three 3″ diameter confocal cathodes
  • 2 RF power supplies
  • Switchable DC power supply
  • Co sputter capable
  • Reactive sputtering available (Nitrogen or Oxygen)
  • 6″ Diameter stage
  • Substrate rotation
  • +/- 10% Uniformity
  • Cryo and turbo pumped to 1 x 107 Torr
  • Substrate heat up to 200 C
  • Liftoff deposition with sputter power
  • Argon pressure range 3-15 mT controllable with 200 sccm MFC controller (no APC valve)

Targets Available

 

 

Target Material Target Purity (%) Diameter (in) Thickness (in) Power Type) Power Max (W) Expected Rate @ 50W Sheet Rho
Aluminum (Al) 99.95 3 0250 DC 300 TBD TBD
Chromium (Cr) 99.95 3 0250 DC 300 TBD TBD
Copper (Cu) 99.95 3 0250 DC 300 TBD TBD
Germanium (Ge) 99.95 3 0250 DC 300 TBD TBD
Gold (Au) 99.95 3 0250 DC 300 TBD TBD
Indium (In) 99.95 3 0250 DC 300 TBD TBD
Iron (Fe) 99.95 3 0250 DC 300 TBD TBD
ITO (Indium Tin Oxide) 99.95 3 0250 DC 300 TBD TBD
Molybdenum (Mo) 99.95 3 0250 DC 300 TBD TBD
Nickel (Ni) 99.95 3 0250 DC 300 TBD TBD
Niobium (Nb) 99.95 3 0250 DC 300 TBD TBD
Palladium (Pd) 99.95 3 0250 DC 300 TBD TBD

 

Diameter (in) Thickness (in) Power Type Power Max Expected Rate @ 50W (Å/s)
Gold (Au) 3.0 0.125 DC TBD TBD
Indium (In) 3.0 0.125 DC TBD TBD
Iron (Fe) 3.0 0.062 DC TBD TBD
ITO (Indium Tin Oxide) 3.0 0.250 DC TBD TBD
Molybdenum (Mo) 3.0 0.250 DC TBD TBD
Nickel (Ni) 3.0 0.062 DC TBD TBD
Niobium (Nb) 3.0 0.250 DC TBD TBD
Palladium (Pd) 3.0 0.125 DC TBD TBD
Platinum (Pt) 3.0 0.125 DC TBD TBD
Silicon (Si) 3.0 0.250 RF TBD TBD
Silicon Dioxide (SiO2) 3.0 0.125 RF TBD TBD
Silver (Ag) 3.0 0.125 DC TBD TBD
Tantalum (Ta) 3.0 0.250 DC TBD TBD
Tin (Sn) 3.0 0.125 DC TBD TBD
Titanium (Ti) 3.0 0.250 DC TBD TBD
Titanium Dioxide (TiO2) 3.0 0.125 RF TBD TBD
Tungsten (W) 3.0 0.250 DC TBD TBD
Vanadium (V) 3.0 0.250 DC TBD TBD
Zinc (Zn) 3.0 0.125 DC TBD TBD
Zinc Oxide (ZnO) 3.0 0.250 RF TBD TBD
Zirconium (Zr) 3.0 0.250 DC TBD TBD

Materials allowed by NMR.

Materials may need special processing requirements see SOP and Design a Process applications for details.

  Year Approved Substrate Material
2026  CMN is Copper Manganese Nickel Oxide (spinel).
2026  CFY is a Chromium-Iron alloy with trace amounts of Yttrium

Training Video: https://www.youtube.com/watch?v=-kzvwDqwa9c&feature=youtu.beProcess Information

Sputtering vs. evaporation overview:

DC Sputtering, RF Sputtering, and E-beam Evaporation are three of the most widely used Physical Vapor Deposition (PVD) techniques in semiconductor fabrication, optics, and material science. While they all deposit thin films, they differ fundamentally in how they vaporize material, their process conditions, and the resulting film characteristics

  • DC (Direct Current) Sputtering: A plasma-driven, momentum-transfer process. A constant DC voltage accelerates inert gas ions (usually Argon) into a target material. The physical impact knocks target atoms free, which then travel and condense on the substrate. 
  • RF (Radio Frequency) Sputtering: Operates similarly to DC sputtering but replaces the constant voltage with a high-frequency AC field (typically 13.56 MHz). This alternating polarity prevents positive charge accumulation on the target, allowing the plasma to stay lit even when using non-conductive targets. 
  • E-beam (Electron Beam) Evaporation: A thermal vaporization process. An electron gun generates an intense beam of electrons focused into a crucible pocket. The kinetic energy melts or sublimes the source material locally, causing it to evaporate and travel upwards to condense on the substrate in a clean line of sight.

Comparison of Key Features

Feature DC Sputtering RF Sputtering E-beam Evaporation
Primary Mechanism Physical momentum transfer (ion bombardment) Physical momentum transfer (ion bombardment) Thermal evaporation (localized e-beam heating)
Material Types Conductive metals only (e.g., Al, Ti, Cu, Au) Both conductive and insulating dielectrics (e.g., SiO₂, Al₂O₃) Refractory metals, precious metals, and oxides
Vacuum Level Medium vacuum (1 to 100 mTorr Ar plasma gas) High-medium vacuum (0.5 to 10 mTorr Ar plasma) Ultra-high vacuum (10⁻⁶ to 10⁻⁹ Torr, no process gas)
Deposition Rate High Low to very low Very high (excellent for thick films)
Step Coverage Conformal (coats sidewalls and complex topography) Conformal (coats sidewalls and complex topography) Directional (poor step coverage, line-of-sight)
Lift-Off Process Poor (coats resist sidewalls, causing tearing) Poor (coats resist sidewalls, causing tearing) Excellent (leaves sidewalls clean for easy removal)
Film Purity Moderate (trapped Argon gas possible) Moderate (trapped Argon gas possible) Excellent (ultra-pure, crucible remains cool)
Adhesion & Density Excellent (high energy atom arrivals) Excellent (high energy atom arrivals) Moderate (often requires a thin adhesion layer)
Alloy Fidelity Excellent (transfers exact target composition) Excellent (transfers exact target composition) Poor (components evaporate at different rates)

Key Engineering Decision Factors
    • When to choose DC Sputtering: When you need fast, highly adherent, and dense metal coatings over broad substrate areas, such as creating barrier layers or conductive interconnect tracks. 
    • When to choose RF Sputtering: When your film target is an insulator or dielectric material, and you require uniform, stress-controlled films where high throughput is less critical. 
    • When to choose E-beam Evaporation: When you are performing lift-off lithography, need to deposit exceptionally pure films, want to quickly build up thick layers, or are working with expensive precious metals (like Gold or Platinum) where a highly focused beam reduces target inventory waste.


SOP:Denton Discovery 18 SOP